Tianli's ternary precursor oxidation and cooling complete system with good sealing effect and without leakage of air and powder, and the oxygen content in the rotary kiln can reach more than 97% stably. At the same time, reliable inner surface processing technology can effectively prevent the incorporation of metal foreign matter.